Engineering

We fix the part, then we print it

Most files that reach us were drawn for another process. The prototype stage is where that shows. We 3D print samples, break them, and redraw the part before it goes into mass quantities. Two recent examples, with the models and the drawings we worked from.

Case 01 · Door hardware

Dust boxes that stopped cracking

A set of twelve door dust boxes for a villa project, drawn with 1 mm walls. The first samples cracked where the floor meets the side walls. We kept every outside dimension, so the parts still fit the same routed slots, and moved material to where it broke.

Rendered from the production CAD
Drag to rotate

What we changed

  • Walls1.0 mm at the face, tapering to 1.6 mm at the bottom
  • Corner2 × 2 mm chamfer where the walls meet the floor
  • Floor1.0 mm to 2.0 mm
  • Bridge12 mm down to 6.8 mm when printed flange-down
  • OutsideUnchanged. 18 mm flange, 14 mm body, 12 mm opening

Printed in ASA, flange face down, so the layers run along the walls. Press Cut open on each version to compare the section.

Squeeze test · before and after

Push on the side walls of both versions with the same force. Drag the slider or run the test.

R1 · as drawnNo load
R1 V3 · strengthenedNo load

An illustration built on a simple beam estimate from the two sections, with the load that cracked the R1 samples taken as 100%. The thicker, chamfered corner of V3 carries about a third of the stress for the same squeeze. It is not a lab test.

Drawing · section through the body
R1 · AS DRAWNSECTION THROUGH THE BODY, AS PRINTEDPRINT BED18 FLANGE14 BODY2412 BRIDGEWALL 1.0FLOOR 1.0CRACKED HERER1 V3 · STRENGTHENEDSAME OUTSIDE, MORE MATERIAL WHERE IT BROKEPRINT BED18 FLANGE14 BODY246.8 BRIDGEWALL 1.0 → 1.62 × 2 CHAMFERFLOOR 2.012 OPENING, UNCHANGED
Drawing · end tab, older revision

On the older design the long, thin end tabs snapped at the body. A 3 × 3 mm gusset under each tab spreads the load.

OLD REV · PLAIN TAB15 TAB2BODYSNAPPED HEREV2 · GUSSETED TAB15 TAB2BODY3 × 3 GUSSET, FULL WIDTH
Case 02 · Facade

A drain cap for a UPVC facade

An 8 mm drain hole in a 5 mm UPVC plate needed a cap that hides the hole, stays in outdoors, and still lets water out. We drew several ways of holding it in place and test-printed them in PETG to compare fit by hand.

Rendered from the production CAD
Drag to rotate

Five ways to hold a cap

  • ACrush ribs that bite into the hole wall
  • BLong snap legs that spring out behind the plate
  • CSplit stem, locked open by a centre pin
  • A3Tapered stem with an open drain path
  • ESoft flap in TPU that seals and still drains

Each cap is 14 mm across. Press Print it to watch a variant build layer by layer.

Drawing · each variant seated in the plate
A · CRUSH-RIB PLUGB · LONG SNAP LEGSC · SPLIT STEMA3 · TAPERED, OPEN DRAINE · SOFT FLAP, TPUØ85UPVC PLATE, OUTSIDE FACE UP
Studio renders

The same parts, up close

Rendered from the production CAD at print layer height. Photos of the finished parts go here as each job ships.

Tapered drain cap in white PETG, showing the layer lines
Drain cap A3 · PETG · 0.12 mm layers
Strengthened dust box cut in half, showing the tapered walls and chamfer
Dust box R1 V3 · cut through the body
Soft flap drain cap in orange
Drain cap E · soft flap
Dust box with gusseted end tabs in black
Dust box V2 · gusseted tabs

Have a part that keeps breaking?

Send the file and tell us where it fails. We'll come back with a fix and a quote.